Modeling of crystallization process of continuously casted strip of aluminium Al 99.5 on the type '3c' installation / Modeliranje procesa kristalizacije kontinuirano livene trake aluminijuma Al 99.5 na uređaju tipa '3c'
(Beograd : Kriminalističko- policijska akademija, 1998)
Studying of processes connected with continuous casting is equally important from technical, economical and technological aspect. All of the previous experimental research [1,2] had shown functional connection between ...
Analysis of the amount of input heat during welding and its influence on structure and toughness of high strengthened micro-alloyed steels / Analiza unesene količine toplote pri zavarivanju i njen uticaj na strukturu i žilavost mikrolegiranih čelika povišene čvrstoće
(Beograd : Kriminalističko- policijska akademija, 1997)
Compared to the low-carbon and low-alloyed constructive steels, application of high strengthened steels has significant advantages. Those advantages are contained in reducing the mass of construction, increasing the carrying ...
The influence of different factors on appearance of accicular ferrite structure in weld metal / Uticaj različitih faktora na pojavu acikularne feritne strukture u metalu šava
(Beograd : Kriminalističko- policijska akademija, 1999)
We are going to analyze a welded joint (weld metal) as a part that connects the segmentic constructions, because welded joints are critical spots in these constructions. Mechanical characteristics and impact ductility of ...