CVD Diamond films produced from hydrocarbons by use of the flat flame method

Link to this page

info:eu-repo/grantAgreement/MESTD/Technological Development (TD or TR)/34022/RS//

CVD Diamond films produced from hydrocarbons by use of the flat flame method (en)
Синтеза дијамантских превлака из пламена угљоводоника техником равног пламена (sr)
Sinteza dijamantskih prevlaka iz plamena ugljovodonika tehnikom ravnog plamena (sr_RS)
Authors

Publications

Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures

Gligorijević, Bojan R.; Vilotijević, Miroljub N.; Šćepanović, Maja J.; Radovanović, Radovan; Radović, Nenad

(Association of Chemical Engineers of Serbia, 2017)

TY  - JOUR
AU  - Gligorijević, Bojan R.
AU  - Vilotijević, Miroljub N.
AU  - Šćepanović, Maja J.
AU  - Radovanović, Radovan
AU  - Radović, Nenad
PY  - 2017
UR  - http://jakov.kpu.edu.rs/handle/123456789/762
AB  - The present study estimated the cracking phenomenon in as-plasma-sprayed hydroxylapatite coatings (HACs) after they were being subjected to the severe cutting conditions in the direction perpendicular to the coating/substrate interface. In order to evaluate the effects of substrate preheating on the occurrence of micro-cracks, the HACs were deposited at different initial substrate temperatures (T-S = 20, 100 and 200 degrees C). The changes in phase composition and HA splat morphology with T-S were observed and were correlated with the cracking occurrence. The results showed that severe cutting conditions introduced a localized cracking in the regions of HACs dominantly attributed to the brittle hydroxyl- deficient amorphous calcium phosphate (ACP) phase. This effect was particularly observable in the HACs deposited without preheating of substrate. On the other hand, the preheating of substrate reduced the presence of micro-cracks and caused insignificant changes in the average local phase composition. In HACs deposited with preheating of substrate, the HA splats (of which HACs are composed) were thinner and recrystallized HA regions seemed smaller in size and more evenly distributed. These results implied potentially important roles of the HA splat formation mechanism on the distribution of ACP and recrystallized HA regions in the as-plasma-sprayed HACs and the cracking resistance of HACs.
PB  - Association of Chemical Engineers of Serbia
T2  - Hemijska industrija
T1  - Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures
VL  - 71
IS  - 3
SP  - 241
EP  - 249
DO  - 10.2298/HEMIND160513034G
ER  - 
@article{
author = "Gligorijević, Bojan R. and Vilotijević, Miroljub N. and Šćepanović, Maja J. and Radovanović, Radovan and Radović, Nenad",
year = "2017",
abstract = "The present study estimated the cracking phenomenon in as-plasma-sprayed hydroxylapatite coatings (HACs) after they were being subjected to the severe cutting conditions in the direction perpendicular to the coating/substrate interface. In order to evaluate the effects of substrate preheating on the occurrence of micro-cracks, the HACs were deposited at different initial substrate temperatures (T-S = 20, 100 and 200 degrees C). The changes in phase composition and HA splat morphology with T-S were observed and were correlated with the cracking occurrence. The results showed that severe cutting conditions introduced a localized cracking in the regions of HACs dominantly attributed to the brittle hydroxyl- deficient amorphous calcium phosphate (ACP) phase. This effect was particularly observable in the HACs deposited without preheating of substrate. On the other hand, the preheating of substrate reduced the presence of micro-cracks and caused insignificant changes in the average local phase composition. In HACs deposited with preheating of substrate, the HA splats (of which HACs are composed) were thinner and recrystallized HA regions seemed smaller in size and more evenly distributed. These results implied potentially important roles of the HA splat formation mechanism on the distribution of ACP and recrystallized HA regions in the as-plasma-sprayed HACs and the cracking resistance of HACs.",
publisher = "Association of Chemical Engineers of Serbia",
journal = "Hemijska industrija",
title = "Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures",
volume = "71",
number = "3",
pages = "241-249",
doi = "10.2298/HEMIND160513034G"
}
Gligorijević, B. R., Vilotijević, M. N., Šćepanović, M. J., Radovanović, R.,& Radović, N.. (2017). Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures. in Hemijska industrija
Association of Chemical Engineers of Serbia., 71(3), 241-249.
https://doi.org/10.2298/HEMIND160513034G
Gligorijević BR, Vilotijević MN, Šćepanović MJ, Radovanović R, Radović N. Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures. in Hemijska industrija. 2017;71(3):241-249.
doi:10.2298/HEMIND160513034G .
Gligorijević, Bojan R., Vilotijević, Miroljub N., Šćepanović, Maja J., Radovanović, Radovan, Radović, Nenad, "Cracking caused by cutting of plasma-sprayed hydroxyapatite coatings and its relation to the structural features of coatings deposited at different initial substrate temperatures" in Hemijska industrija, 71, no. 3 (2017):241-249,
https://doi.org/10.2298/HEMIND160513034G . .